making mould for defuser


Author
Message
Ronny
Ronny
Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)Supreme Being (598 reputation)
Group: Forum Members
Posts: 58, Visits: 401
Sam: looking forward to see the results, im considering making some diffusers myself.

MarkMK: Do you have any photos of the mould(s) you used?
MarkMK
MarkMK
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Apologies for using the links, but it won't let me add any pics directly on here for some reason

https://www.dropbox.com/s/0horv6qigmjuf1s/20160307_141955.jpg?dl=0

https://www.dropbox.com/s/xncr74e52etz9x4/20160307_142003.jpg?dl=0
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Dropbox does not allow direct hotlinking so you can't even use the image tags.
I just upload to google photos and hotlink directly from there cache Wink