Hello all,
I wrote late last year and asked if assistance could be give to make a mould for a F3 defuser. race car. and that a couple of attempts had been made with a sad ending, and too the rubbish heap they went.
I have made a mould off the old defuser using glass etc. and I thought I would use this as a mould for the defuser however, my troubles began when I used foam and carbon fiber to form the underneath ribs and when it was pulled down with the vacumm bagging process the ribs become out of shape under pressure.
I am no expert with this process and I would appreciate assistance?.
Do you have to have a split mould top and bottom to form the mould.
I would appreciate your comments, I will take a photo tomorrow and post it until then
Thanks
Sam
By davro
-
3/7/2016 9:39:36 PM
Dropbox does not allow direct hotlinking so you can't even use the image tags.
I just upload to google photos and hotlink directly from there cache
Mould looks nice!