Adhesive epoxy cf to steel?


Author
Message
Davidpetty1988
Davidpetty1988
Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Any idea what adhesive to use on epoxy infused carbon fibre to stainless steel?
Thanks 
Dave
Edited 10 Years Ago by Davidpetty1988
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Use a structural epoxy adhesive like Araldite 2014, or Easy Composites ET500. Alternatively, I'm a big fan of methyl methacrylate adhesives like SAE or EC's Voodoo Glu. 

Surface prep is paramount. You need to key both the carbon and the steel very well, and clean with acetone very well. If you are bonding to a peel ply surface, then just clean it with acetone before bonding.  
Davidpetty1988
Davidpetty1988
Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Cheers hanaldo

Dave
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search