moisture Pickup in Carbon cloth


Author
Message
D3O Phil
D3O Phil
Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)
Group: Forum Members
Posts: 22, Visits: 498
Hi Quick question

Is carbon cloth subject to picking up moisture while it is being stored? should I be storing it in a warm environment before laying up so that the material stays dry?

what sort of issues could I see if the cloth was left out in a workshop/shed before lay up.

All for resin infusion but I guess this question will be applicable to hand layup too.

Phil
Reply
D3O Phil
D3O Phil
Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)Supreme Being (265 reputation)
Group: Forum Members
Posts: 22, Visits: 498
Hi Warren

many thanks I suspected there would be some effect on the resin if using a fabric which had been left out. but it is good to be confirmed,

Is there any ideal storage condtions to keep the fabric in prior to use?

Phil