By D3O Phil - 2/23/2016 10:24:08 AM
Hi Quick question
Is carbon cloth subject to picking up moisture while it is being stored? should I be storing it in a warm environment before laying up so that the material stays dry?
what sort of issues could I see if the cloth was left out in a workshop/shed before lay up.
All for resin infusion but I guess this question will be applicable to hand layup too.
Phil
|
By D3O Phil - 2/24/2016 2:43:13 PM
Hi Warren
many thanks I suspected there would be some effect on the resin if using a fabric which had been left out. but it is good to be confirmed,
Is there any ideal storage condtions to keep the fabric in prior to use?
Phil
|
|