Hi to all, just a quick question or two on peoples opinions and methods that they use for finishing there parts.
I already have a fairly glossy finish after demoulding.
So...
  1.  On my first test peice I intend to use a clear automotive laquer from a spray can. Any input on what grit sand paper pre and post laquer and how many coats much appreciated.
  2. On my second I wish to use easygloss polishing compound once again any input on pre sanding application grits or anything like that or tips for applying the easygloss.
  3. Just bare no coating just a sanded finish tip on grits and what not.
  4. And lastly any other ideas that anyone put forward would be great such as gel coating or any thing else.
Thank you in advance

Keep on carboning
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The Easygloss is very straight forward, just follow the instructions on the bottle. I do find it works better when applied with a soft pad on a RO polisher, but by hand works too. 