Hi, 

Newbie here. I am trying with making a part and i can't get rid of the bubbles. 



I usually get a lot of small voids and few huge bubbles. I prepare the mould with 5 coats of buffed wax (Axel PasteWiz) and a layer of PVA for a sure release. I heat the mould with a hot air gun and also heat the mixed resin and hardner. Then i apply 6 layers of carbon fibers, heating in between every layer. 

Any idea what I am doing wrong?
Reply
GordonFreeman
GordonFreeman
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 2, Visits: 57
Should I roll it right after putting down an other layer?

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search