Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I agree with the other posters .. Small parts with tight corners do not mix well with medium weight cloth/fabric and wet -lay ..
As soon as you have vacuum or infusion, and prepare your "stack" well, most of the bridging and trapped air will not be a problem.
To wet lay small parts with small radius corners, you really do need to use light weight CF cloth - Also Plain weave is harder to get to follow complex shapes and compound curves than Twill weave.