Surface requirement for mould making
Surface requirement for mould making
Post Reply
Like
7
Prev
1
2
Jump To Page
Surface requirement for mould making
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
kidpaint
kidpaint
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 676
Actually primer is porous. Thats why they require a top coat as a color and protective layer. You are right that paint alone wont stick to metal and the primer is there to help adhesion. This is why when metal is left in primer it can still rust. In my painting course we are always taught to never leave anything in primer esp if it is going to be out in the elements.
If you are using a 2 part paint system, if the catalyst is mixed correctly then the only thing that can soften it is a paint remover. acetone or thinner once cured shouldnt have any effect.
Reply
Like
5
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I do believe people have long confused the hygroscopic nature of some primers with porosity. Just because a material can absorb moisture does not mean it is porous. Again, this depends on the formulation of the paint. Primers are not intended as protective coatings, they don't have any of these qualities built into them because they don't need it.
However even this, I believe, is no longer really relevant. Old style cellulose primers are likely the culprit, as cellulose is naturally hygroscopic. Hence spray painters have been coached into treating primers as non-sealed substrates, which when you are painting a car for $15,000 does make sense, you follow certain procedures. Polyester primers are a similar story, generally the rule is you ALWAYS dry sand polyester coatings and allow them to cure overnight before commencing wet sanding otherwise they absorb water. That isn't just primers though, it's any polyester coating, and it isn't due to porosity.
I can understand why spray painters have this mindset about primers absorbing moisture; hell if I were spray painting my car I wouldn't leave it in primer either. But in the context of making moulds, a 2k polyurethane is not porous. It will not absorb release agent, it will not absorb gelcoat, it will not absorb anything.
Reply
Like
4
The Fibreglass King
The Fibreglass King
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 69,
Visits: 652
Hanaldo,
Very well put, your advice is always on the ball. You are an asset to this forum.....
Kind Regards
The Fibreglass King
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search