Actually primer is porous. Thats why they require a top coat as a color and protective layer. You are right that paint alone wont stick to metal and the primer is there to help adhesion. This is why when metal is left in primer it can still rust. In my painting course we are always taught to never leave anything in primer esp if it is going to be out in the elements. 

If you are using a 2 part paint system, if the catalyst is mixed correctly then the only thing that can soften it is a paint remover. acetone or thinner once cured shouldnt have any effect. 
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I do believe people have long confused the hygroscopic nature of some primers with porosity. Just because a material can absorb moisture does not mean it is porous. Again, this depends on the formulation of the paint. Primers are not intended as protective coatings, they don't have any of these qualities built into them because they don't need it. 

However even this, I believe, is no longer really relevant. Old style cellulose primers are likely the culprit, as cellulose is naturally hygroscopic. Hence spray painters have been coached into treating primers as non-sealed substrates, which when you are painting a car for $15,000 does make sense, you follow certain procedures. Polyester primers are a similar story, generally the rule is you ALWAYS dry sand polyester coatings and allow them to cure overnight before commencing wet sanding otherwise they absorb water. That isn't just primers though, it's any polyester coating, and it isn't due to porosity. 

I can understand why spray painters have this mindset about primers absorbing moisture; hell if I were spray painting my car I wouldn't leave it in primer either. But in the context of making moulds, a 2k polyurethane is not porous. It will not absorb release agent, it will not absorb gelcoat, it will not absorb anything. 
The Fibreglass King
The Fibreglass King
Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)Supreme Being (833 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hanaldo, 
                Very well put, your advice is always on the ball. You are an asset to this forum.....
Kind Regards
The Fibreglass King
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search