Hi
On my car i have two heatshields where one of them are a tad rusty.
And they are heavy also..
So i figured i should try make them in carbon or twaron or whatever you guys recommend.
But with the high temp resin.

But since it is a car used on trackdays the turbos will generate quite some heat, also since they are working a bit overtime as the car is tuned.

Now two questions.
1. will the part withstand the heat generated? it is really hard measuring the heat due to the placement of the turbo/shield.
2. what happens if the heat is to much? will the resin/carbon ignite?
3. Optionally i have heat reflective goldtape  if thats of any use.

Sorry for the big pictures.

Here is the shield in question
http://i.imgur.com/tuMVcvS.jpg


Thickness 13mm wrench for scale
http://i.imgur.com/MLpChpa.jpg



Distance between  turbo and shield. (the turbo itself is also shielded, i wont mess with that particular part)
You see the part in question just right of the turbo.
http://i.imgur.com/1lHh1lb.jpg
Edited 9 Years Ago by Ronny
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You'll need to get an infra-red thermometer and measure what heat the parts will see. A heat shield sitting right next to the exhaust on a turbocharged track car isn't unlikely to see 200 degrees, which would be too hot for even the high temperature resin. 

That said, I do think the worst that would happen is severe discolouration and potentially cracking. It would take prolonged exposure to extreme heat for the resin to ignite, in which case you would have more serious issues than burnt heat shields. 