Whats available for carbon fiber fabric that comes in different colors, BUT also has a colored...
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
You tried care reinforcements ?
they have a fairly large stock
Reply
Like
5
EVILTL
EVILTL
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 43
You lost me on that one. Im new at this, so im not familiar with all the terms, and not sure how that relates to color?
Reply
Like
4
Dravis
Dravis
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
I think he means some online supplier, but my Google-fu is not strong enough to find it ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
5
EVILTL
EVILTL
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 43
Ahhh..ok. ..I was over thinking his response
Reply
Like
3
EVILTL
EVILTL
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 43
Check out this attachment. The orange chrome skull is what I am trying to match with a carbon fiber weave. The basic oranges that I've found just don't go with it. Like I had mentioned earlier, I'd like to find a cf fabric with more of an orange-chrome look in it, but I still want the black c.f. in it also.
Attachments
Screenshot_2016-01-28-08-09-42.png
(
633 views,
1.00 MB
)
Edited
10 Years Ago by
EVILTL
Reply
Like
4
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Keep in mind that the dry fabrics may appear differently once wet out with resin. I find a lot of the colours end up slightly darker than when they were dry, especially if you've got straight black carbon backing layers behind the surface.
To be honest, I don't think you will find what you are looking for. I would play around with the orange fabrics that you can get and try some resin tints. You may be able to tint the resin enough to make the orange look a bit more like what you're after, without affecting the appearance of the carbon.
Reply
Like
5
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
As Hanaldo said the colours get darker.
This is a part I did with the orange/carbon hybrid fabric and it went a kind of red/brown.
Fastacraft Facebook page
Edited
10 Years Ago by
Fasta
Reply
Like
4
EVILTL
EVILTL
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 43
Your right hanaldo. i dont think theres anything out there exactly like what i want. and very good point about the resin making the colors look a bit darker. I never stopped to think about that, but makes complete sense since that rule seems to apply to other areas such as putting a clearcoat over a base and it slightly changing color perception.
Reply
Like
4
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Carr Reinforcements - they do some really funky weaves, lowish minimum orders
I've got a couple of samples from them that are a V-weave so if you wanted to do a bonnet with the weave mirrored on the centreline, you can do it with a single piece rather than trying to get two lined up perfectly - brilliant!
They also do coloured interwoven, most colours - their website was rather out of date last time I looked but they are well worth a telephone call.
Reply
Like
4
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
theres an italian company that does some very cool stuff too, similar to carr reinforcements. They have a dealer in the north of the uk called cristex
http://www.cristex.co.uk/
http://www.g-angeloni.com/
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search