deceased10 (25/01/2016)
matthieutje65 (25/01/2016)
good job so far! now come the fun part of sanding and recoating :p I have a new video coming online tomorrow on my youtube btw about that topic :p


No way! I may just wait for it then! 


haha :p its about fixing bad parts but in fact it's just like skinning parts using the epoxy coating resin from easycomposites that is now improved and called XCR, you will get better results and work faster this way than coat it with regular epoxy Smile video online at 17:00 Belgian time today (tuesday) on www.youtube.com/matthieutje65 Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Unfortunately I'm not able to buy from Easy composites being in Canada, Stuck using a 2 part epoxy from West Systems.  Every time I put in my cart it says they do not ship dangerous goods to canada. Sad 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
ow to bad...try looking for a thicker epoxy resin...the coating resin is very thick which makes it easier to cover everything in less coats

link to video is here btw 

https://www.youtube.com/watch?v=q8qNwNTjOUA

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
YA THIS stuff is really thin, I almost think I should do a second layer tonight before sanding, so i dont go to the carbon
deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Is it bad to add another layer of resin to a fully cured resin layer? Or should I sand the first coat? Im just scared of sanding into the carbon fiber
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
If fully cured it's better to give it a soft sanding, say 400grid wet and you will see if you go through the fibers or not. Most important thing is that low spots are ok, it's just that you need more coats. Don't try to go through as much low spots as possible when you are sanding, but you need to know where to stop...then you can add more layers wet on dry/tacky thats the chemical bond...if fully cured you will need to sand in between to get a mechanical bond

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
WHATS THE BEST time to trim all my pieces?  I was thinking of trimming all the edges now on the first coat? 
SeftonMitchell
SeftonMitchell
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 34
I am curious as to how this dash turned out for you as I have a dash that is prepped and just about ready to lay on the CF, but my dash is a foam dash, after I removed all the vinyl.
Can you post pics of your finished dash? 
Edited 9 Years Ago by SeftonMitchell
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search