Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
New Member Introductions
»
Newbie in Coventry
Newbie in Coventry
Post Reply
Like
2
Newbie in Coventry
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
stuart321
stuart321
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 178
Hi,
Just starting out with resin infusion to make parts for my rally car and maybe some friends running similar cars.
I've tried a test piece with 1,2,3 layers of CF, kevlar and soric to get a feel for strength of different combos so ready to get started with some proper parts.
2 questions immediately come to mind if those with more experience could comment
- How soon after clamping the infusion line should you clamp off the vacuum line? Intuitively it seems leaving it open for 5-10mins will help draw out excess resin which minimises unnecessary weight. Am I thinking right or are there other considerations?
- How does 200 & 295gsm CF cloth compare for strength? Its 50% more weight but I'm getting the feeling its not 50% stiffer.
Thanks in advance for any pointers and I'm looking forward to sharing details of my progress & hopefully not asking too many stupid Qs
Stuart
Reply
Like
2
Daz
Daz
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 93,
Visits: 651
Hi There,
Im also a residend in coventry,
I usually give it a couple on min before claming the vac line,
I havent experimented witrh different carbon weights
i have found 2 layers of carbon and sorric works fine for me
The roof is plenty strong enough with this layup
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search