Good morning,

I have to build a +- 2.5 liter CF air tank that hold 10 bars continuously.
My plan is to shape a cylinder (7.5 cm diameter and 15cm long) in a block of foam that need to resist epoxy resin under vacuum, wrap it with 6 layers of CF, after cooking I will drill two holes where I will later install some plugs, filling through them acetone to dissolve the foam and get a final clean inside piece.

My questions are :

- is my plan the easiest or do you have a better idea ?
- which foam to use (I want to avoid glue in the process and 10cm height is your only option) ?
- how many layers of 400gr CF would you recommend (my intention is 6) ?

Thanks for your kind advice.

               
Reply
rapidos
rapidos
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 8, Visits: 36
Thanks Dravis for your good comments.

There is also kevlar on the outside layer, but i decided to finish it with one last layer of CF for the esthetic. (CF airbox and tube in the vincinity)

It does not need to be protected from anything as it is covered by the rear clam directly 1mm above it.
My choice to keep the design as close as possible to the original was guided by the only 10mm left clearance I have in length and 1 mm in high and the need to stick as close as possible to the identical volume. The tank is designed to allow 7 gear change and that occurs in one single second so it can't be smaller.
The tank is closed as you see it. I decided to mount the connections as they are on the original, no flange but just 7 steps screwed in with Teflon tape.

I always tend to follow my feelings. A challenge indeed.
Edited 9 Years Ago by rapidos
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
rapidos - 10 Years Ago
Dravis - 10 Years Ago
rapidos - 10 Years Ago
ChrisR - 10 Years Ago
Warren (Staff) - 10 Years Ago
Dravis - 10 Years Ago
rapidos - 10 Years Ago
rapidos - 9 Years Ago
Dravis - 9 Years Ago
rapidos - 9 Years Ago
Warren (Staff) - 9 Years Ago
Dravis - 9 Years Ago
rapidos - 9 Years Ago
ajb100 - 9 Years Ago
Dravis - 9 Years Ago
rapidos - 9 Years Ago
ChrisR - 9 Years Ago
rapidos - 9 Years Ago
ChrisR - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search