Spitfire
Spitfire
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 25
Hi again
Finished a mould using the Vinylester Uni-Mould system. I was going to use wet layup in the moulds but have now decided to use pre-preg instead, so I will need to post-cure the mould.
What is the accepted post-curing procedure for Uni-Mould? i.e: temperatures and dwell times at said temperatures?
Also, could anybody tell me, what is the highest maximum temperature I can SAFELY take the mould up to during post-curing?
Thanks for any help.
Reply
Like
3
Reply
Davo456
Davo456
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 8,
Visits: 77
see here..
https://system.na1.netsuite.com/core/media/media.nl?id=5299&c=3937524&h=6458bc02d742162729a6&_xt=.pdf
top of page 4 -
For ambient temperature use, a post cure of the mould is recommended, but not required. If you intendto use the mould for pre‐preg or in‐mould post curing of your parts then an elevated temperature postcure is required.Recommended post‐cure for elevated temperature mould use:10hrs at 60°C 2hrs at 70°C 2hrs at 80°C 2hrs at 80°C
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Uni Mould post-cure, temp and dwell time.
Spitfire
-
9 Years Ago
see here.....
Davo456
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search