Is anybody using anything other than the type of silicone connectors that EC sell that they can recommend?

I've found that, after half a dozen infusions or so, the excess resin begins sticking to them and they tend to start breaking apart. At around £4 each I wondered if there was a good alternative out there that might just have a bit more longevity?

Thanks

Mark
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I mostly run the tube in without a connector, except on complex parts with an inlet not being on the flange I use the silicone connectors...did more than 20 infusions with the first...Just rub them in with some Chemical release agent Cool

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search