Hello all,
I have a question about printing on carbon fibre. Me and my friends are working on some project and we would need to print something on carbon fibre.

We have already tried UV printers, direct printing and screen printing. The only method that is close to OK is screen printing, but paint just isn't durable enough (maybe if we could apply some kind of varnish over it would be ok).

We heard about some kind of foil, that you apply before curing carbon fibre but we don't know what would be the finish with that technique and what kind of foil we would need.

We are using 200g pre-preg cured at 130 deg C.

Thank you for your help!
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Screen Printing and then lacquer is probably the easiest reasonably durable approach.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matevz - 9 Years Ago
scottracing - 9 Years Ago
Matevz - 9 Years Ago
f1rob - 9 Years Ago
Warren (Staff) - 9 Years Ago
VVS - 9 Years Ago
Colt Parker - 7 Years Ago
scottracing - 9 Years Ago
Matevz - 9 Years Ago
valzine - 9 Years Ago
Batista Wang - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search