Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Printing on carbon fibre
Printing on carbon fibre
Post Reply
Like
11
Printing on carbon fibre
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Matevz
Matevz
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 36
Hello all,
I have a question about printing on carbon fibre. Me and my friends are working on some project and we would need to print something on carbon fibre.
We have already tried UV printers, direct printing and screen printing. The only method that is close to OK is screen printing, but paint just isn't durable enough (maybe if we could apply some kind of varnish over it would be ok).
We heard about some kind of foil, that you apply before curing carbon fibre but we don't know what would be the finish with that technique and what kind of foil we would need.
We are using 200g pre-preg cured at 130 deg C.
Thank you for your help!
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Printing on carbon fibre
Matevz
-
10 Years Ago
you can create stickers and place them into the mould before the carbon and then cure it, this is...
scottracing
-
10 Years Ago
At first thank you very much for fast reply. We are trying to make business card. It is made out...
Matevz
-
10 Years Ago
Made myself a couple of hundred cards years ago mine were 3ply 190 gram and I had all my details...
f1rob
-
10 Years Ago
Screen Printing and then lacquer is probably the easiest reasonably durable approach.
Warren (Staff)
-
10 Years Ago
My best friend is a fishing rod builder and uses water soluble screen print decals for writing,...
VVS
-
10 Years Ago
Hello! I am also trying to figure this process out and was wondering if you could provide just a little more info to help me get started. I took a look at the rods and am really impressed. Is there a...
Colt Parker
-
8 Years Ago
http://www.aerodynamix.co.uk/carbon-engraving.html another way to do it, if the sheet is thick...
scottracing
-
10 Years Ago
Thank you all for the answers! VVS: at first I must say those fishing rods look fantastic. If I...
Matevz
-
10 Years Ago
I was able to achieve good results by creating vinyl stencils (you can cut them by using any kind of...
valzine
-
10 Years Ago
According to my acknowledge and experiences, Laser printing is one of the best way to print on carbon fiber (tube or plate or whatever with a smooth surface) Weeks ago, we'd conducted an experiment.....
Batista Wang
-
6 Years Ago
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search