Hello all,
I have a question about printing on carbon fibre. Me and my friends are working on some project and we would need to print something on carbon fibre.

We have already tried UV printers, direct printing and screen printing. The only method that is close to OK is screen printing, but paint just isn't durable enough (maybe if we could apply some kind of varnish over it would be ok).

We heard about some kind of foil, that you apply before curing carbon fibre but we don't know what would be the finish with that technique and what kind of foil we would need.

We are using 200g pre-preg cured at 130 deg C.

Thank you for your help!
Reply
valzine
valzine
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 6, Visits: 21
I was able to achieve good results by creating vinyl stencils (you can cut them by using any kind of cutting printer like silhouette portrait), applying them on carbon fiber, and then sandblasting the area. I then degrease it and paint it over with any automotive paint, then a layer of clear coat. Remove the vinyl, polish the area, and it will stay forever. You could also use a primer before painting, but in my case it didn't need it. Hope this helps
Edited 9 Years Ago by valzine
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matevz - 9 Years Ago
scottracing - 9 Years Ago
Matevz - 9 Years Ago
f1rob - 9 Years Ago
Warren (Staff) - 9 Years Ago
VVS - 9 Years Ago
Colt Parker - 7 Years Ago
scottracing - 9 Years Ago
Matevz - 9 Years Ago
valzine - 9 Years Ago
Batista Wang - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search