Took my 3mm thick FC plate to fablab where they have nice cnc router, wanted to cut out some arms for quadcopter frame. All went well but the router bits did not last long. I never used that sort of machine before, so i have few questions, first of what kind of bit i should use for CF ?
How about the rpm ? and speed ? 
Any info regarding to this topic is appreciated 

thanks  
Reply
taikuri
taikuri
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 13, Visits: 167
Hi.

thank for all the tips. i dont have access to waterjet, so i will continue with this method.

i did order something similar to these router bits and will give it a try once im back home from x-mas vacation.
Blackrat (18/12/2015)
http://www.ebay.com/itm/Kent-10-Fishtail-3-0mm-Diameter-Carbide-Router-Bits-End-Mill-and-Engraving-Burrs-/291486224465?hash=item43ddeed051:g:emoAAOSw~OdVdGH-

you need to use a 'burr' if you in a hurry and cant wait for shipping , then use a tile cutting bit  ...