First off... do you know what the back side looks like? The "thickness" seems to me to be a different part then the metal cover? some of the engines I've seen with cam-chain covers use a fibre part against the engine block + a thin metal cover on top of that, usually the "fibre" part has cutouts to leave room for the internal moving parts..
You really need to remove the cover and take a closer look at it .. you may well have a more complex part than just a flat 8 mm thick cover ..
I have managed to make quite nice cosmetic parts (End caps for Bike exhausts + exhaust shields) with the EC high temp resin ..
It need a "stepped" postcure to reach the 180 degree Tg .. this can be found on the sheets for the EC resin.