Im looking for some advice on how to make the part below and mould?

It is a cam chain sprocket cover on a small 160cc engine, Dead flat and 8mm thick..

Is this even possible with the heat/oil?? 





Reply
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
The max temp it gets is 130 deg C so you wasn't far off.

That sounds like a really simple process..will the surface be pin hole free?

Should i oven cure , then post cure up to the 130 deg C?