67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I have a mould that i cleaned with the mould cleaner. Then I applyed easy lease, apx 7 coats.
i used a brush to apply the G50 gelcoat. I could not get a even coat, because i got holes in the coat. Looked like the mould had been contaminated by chemicals, but iam shure it isnt. The gelcoat cured for a couple of hours before i took i of. Iam cleaning again with the mould cleaner but it dont seem to evaporise like it i remember it does. It still look like the mould is contaminated.
Any ideas?
Reply
Like
2
Reply
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yes mould cleaner will remove the Easylease. You shouldn't need to use mould cleaner anyway, there's no issue with what is on your mould. The issue is that you are trying to apply a liquid to a surface with very little energy, so the liquid adheres to itself easier than it adheres to the surface. This causes the droplets of liquid to form the shape that requires the least amount of surface area, a sphere or 'bead'.
There's no easy solution for this as it's a simple physics issue. The best solution is to spray the gelcoat. If you have an area where you can spray, borrow or buy a compressor and a cheap HVLP gun (preferably with a 2.0-2.5mm tip). Then the technique that Alex described works perfectly and is the best way of applying an in mould coating.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Problem when I apply gelcoat to the mould
67redrocket
-
10 Years Ago
It is contaminated; by the release agent. That's a common issue with chemical release agents, they...
Hanaldo
-
10 Years Ago
This is the age old problem! The better the release, the more likely it is to create such a high...
alex.mc
-
10 Years Ago
I did a new try. Cleaned the mold with the EC mouldcleaner. Then three coats of easy lease and then...
67redrocket
-
10 Years Ago
Yes mould cleaner will remove the Easylease. You shouldn't need to use mould cleaner anyway, there's...
Hanaldo
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search