I have a mould that i cleaned with the mould cleaner. Then I applyed easy lease, apx 7 coats. 

i used a brush to apply the G50 gelcoat. I could not get a even coat, because i got holes in the coat. Looked like the mould had been contaminated by chemicals, but iam shure it isnt. The gelcoat cured for a couple of hours before i took i of. Iam cleaning again with the mould cleaner but it dont seem to evaporise like it i remember it does. It still look like the mould is contaminated. 

Any ideas?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search