Hi All,

I have a few kayaks which the gel coat has come off and they are now porous.  Has anyone any recommendations for paint that can be easily applied to the surface?  We have used 2 pack polyurethane in the past but I have heard that it is nasty stuff to use without an air fed mask.

They are both epoxy and kevlar constructions which is why he polyester gel falls off them after 10 years or so.

Edited 10 Years Ago by panda
Moranatang
Moranatang
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 17
Durepox is what you need