Hi All,

I have a few kayaks which the gel coat has come off and they are now porous.  Has anyone any recommendations for paint that can be easily applied to the surface?  We have used 2 pack polyurethane in the past but I have heard that it is nasty stuff to use without an air fed mask.

They are both epoxy and kevlar constructions which is why he polyester gel falls off them after 10 years or so.

Tom
By Moranatang - 10/8/2015 11:10:09 PM

Durepox is what you need