I'm planning on infusing some sandwich panels that will be 1 outer skin of 200gsm carbon 5mm perforated PVC core and 1 inner skin of 200gsm carbon. Will it negatively influence my infusion if I only put peelply on the inner skin (bag side) where I plan on doing secondary bonding? The whole thing would have a layer of P3 film and flow medium on top of it.
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Honestly, 50mm centres is plenty. How big is the infusion? 
nc42
nc42
Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)
Group: Forum Members
Posts: 23, Visits: 365
around 3m2, long and skinny. With any luck it will resemble fasta's avatar picture....
Edited 10 Years Ago by nc42
nc42
nc42
Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)Supreme Being (181 reputation)
Group: Forum Members
Posts: 23, Visits: 365
Resemble, but not as pretty or fast...
Edited 10 Years Ago by nc42
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search