As a home builder working in a non heated garage ive got a system going that's working well.
I do the plug work in the week and then come Friday I start the mould.
Friday evening I put the first tooling coat on, this is followed by a second coat Saturday morning,
Saturday tea time I couple coat and then Sunday lay down the final resin.
If its warm you can work outside, if its cold I heat the immediate work area with a cheap halogen heater, only needs to be running at 400watts so cheap and everything is curing well.
I'm catalyzing at the top end of the recommend levels and getting it down fast, only mixing 200 to 300 grams per mix.👍
|