Hi folks,



Just a quick explanation of my current project. And a chance for me practice my skills at uploading pictures  Smile

This is what I'm trying to make. The rough shape of the quad headlight cover was vacuum formed using my DIY vacuum former.





I'm still a long way away from creating the final product, I know. But a lot of things have changed since then. Namely the mounting brackets. The new design is a modular system, these plugs are made of MDF, I've had to use body filler to shape the draft angles, as I'll be using my newly acquired Formech 508DT vacuum forming machine.

Here are my MDF plugs for the headlight brackets >>







My first question to you guys would be, now that I've purchased some 'Pattern-Coat Primer' to cover the plugs with, is how to measure out ( or weigh ) how much pattern-coat primer I need the cover the plugs ?

Would I calculate the volume of the plug ? say, L x W x H ........ then what  ?



Reply
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Many thanks Dravis,

My MDF plugs are ready, all flatted, sanded, just ready for the Pattern-Coat Primer.

They're basically box shaped. 

(L)150mm x (W)140mm x (H)70mm

So I have to workout the volume of said part.

V=L x W x H ( V=15x14x7 ) to get the volume area in cm3

the total is 1470 cubic centimetres



I then converted that volume into weight and got 52 fl.oz ( imperial )

That's an awful lot of resin just for a small plug, that's over 2 pints per plug !

This is what I'm covering with one layer of resin >>



There's two in the picture, but in all I have four as they're modular construction. But I'll be doing them individually.
I'll apply more coats of resin if required.







TURK


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 10 Years Ago
Dravis - 10 Years Ago
TURK - 10 Years Ago
Dravis - 10 Years Ago
TURK - 10 Years Ago
Dravis - 10 Years Ago
Dravis - 10 Years Ago
TURK - 10 Years Ago
Rich (Staff) - 10 Years Ago
TURK - 10 Years Ago
Rich (Staff) - 10 Years Ago
Dravis - 10 Years Ago
TURK - 10 Years Ago
Rich (Staff) - 10 Years Ago
TURK - 10 Years Ago
Dravis - 10 Years Ago
TURK - 10 Years Ago
TURK - 9 Years Ago
TomDesign - 9 Years Ago
TURK - 9 Years Ago
Nightfox - 9 Years Ago
TURK - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search