Hi all,

This is my very first post...

I'm thinking of buying an autoclave. I have only received a few pictures so far.
It's 2 meter long  and 0.9 m i diameter (inside). It's probably only approved for 3 bar.
50 years old and used for vacuum and steam threatment at a yarn factory, I think...
I will probably have to redo a lot to make it work.
Price: ~£500. What do you think.

PS I have no experience of prepreg and autoclave so far ;-)

Best Regards,
Magnus
Attachments
koenig.jpg (2 views, 672.00 KB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I'd give it a miss then. Build yourself a simple oven with a good PID controller and get into OOA pre-pregs. It's great stuff, exceptionally easy to use and you won't waste the time and money you would trying to repurpose that autoclave. 