Anybody have any tips to get minimal wrinkles when shrink wrapping tubes?

I don't have wrinkles when i wrap the tube, just once its heated
Replies
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi, could you explain a little about how you are working, are you applying heat with a gun,heater,oven etc.
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Im using steel tube as mandrel, wet lay up with 3k braided sleeve then wrapping with shrink tape.

Then putting it in an oven at 130 degrees C 