posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 155
Hello,
my friend asks me to make a simply heat shielding for his air filters in motor bay (Nissan 370Z/Fairlady Z34) But it is carbon good material for shields? I can't find infos about it.
Thank you for your advices
-------------------Amateur from one little garage ----------Sorry for my English ----------------------------------------------
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
It works ok for the sort of temperatures you see in an engine bay. What does work well is if you make a carbon sandwich laminate with a core that has good thermal insulation properties, like cork.
Reply
Like
3
Pustil
Pustil
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 155
Thank you, I'll try it...
-------------------Amateur from one little garage ----------Sorry for my English ----------------------------------------------
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search