Female canoe mold difficulies


Author
Message
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yes ... Plugs can be a lot of work ... But a really well made plug saves so much work on the rest of the process!

When you go ahead and make a LARGE project like this, everything gets "amplified" .. BigGrin  (especially the time needed)

.. But with a good mould made from the plug, you can start up a production of the canoes...

Maybe make a bit of money to make up for all the work  Smile

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Zedok
Zedok
Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)
Group: Forum Members
Posts: 18, Visits: 115

After a winter lull, I recently got back inthe workshop. The pattern is having its first pattern coat primer. Still lotsof work to do before starting to make the mould itself. 


Attachments
canot_mai_2015.jpg (506 views, 209.00 KB)
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Looking good Smile

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Zedok
Zedok
Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)
Group: Forum Members
Posts: 18, Visits: 115
Hi all. Well my pattern is finished and I have applied a coat of Pattern-Coat Hi-gloss.  Here are my issues: 
1) Although the resin is supposed to have good self-leveling properties, I notice that there are unevenness when applied. This requires additional sanding with 120 or 180 grit paper (Picture 1 shows partly sanded side surface of the pattern).  
2) There are little depressions on the gloss surface approximately 1-2mm diameter. I assume they are popped little bubbles (Picture 2). 
I was careful not to add air in the resin whilst missing and I used a reasonably good brush. Are these issues due to the type of brush that I used? Have I applied the resin too quickly too much at one time? Anyhow, I did not expect to have have to go back down to 180 or 240 grit after the gloss. 
Any comments on where I am going wrong?
Thanks.
Attachments
Picture 1.JPG (503 views, 1.00 MB)
Picture 2.JPG (508 views, 1.00 MB)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's very difficult (ie. virtually impossible) to get a smooth finish when brushing a coating, it will always be uneven no matter how well it self levels. The small holes are likely to be air as again, it's difficult to brush a coating without trapping even a small amount of air. That said, it is also possible it is solvent outgassing, of which you can do very little about. Fortunately, it's easy to fill these little holes and sand smooth. 

Unfortunately, there is no real easy solution to the task unless you can spray your coatings. If you have the equipment and ability to spray, this will greatly reduce the amount of sanding work you need to do. If you can't spray, then you are committed to a lot of sanding hours, and you'll have to accept that you CAN'T go for the quick option of sanding down with 120. You will need to sand down with 320-400 until flat, which will take a long time. On such a large job, an orbital sander wouldn't be a bad investment. 

It's simply a case of sanding and coating and sanding and coating until you can get the surface flat without rubbing through the coating. Then you can move through the wet sanding stages and finally compound. It's the worst part of the job and I don't envy you for the size of your task, but it's a great feeling when you're finished! 
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I've just finished a plug and a mould for a GSXR Dragbike tank cover, I had the same issues with the High gloss Pattern coat, stripey and rather uneven, even on top of a completely flatted down cover of Pattern Coat primer.
(I can paint 2-K  boat varnish with the type of brush I used, to a level that looks like it is sprayed on ... I've had years of practice on boats ...)

I also had to use 240 grit on a circular sander to speed up my work.. I had to sand so much down that i broke through the high gloss i a few small places, so I decided to try spraying the High Gloss, using the Gel-coat cup gun.. That actually worked MUCH better, the second coat was much smoother  BigGrin But it still had som areas of "orange peel texture"   I sanded this down using dry 400 grit, then went up to 1500 wet sanding .. I Polished only with coarse compound, since I wanted a satin finish in the plug and mould.  The (Unimould) mould came out very nice, even though I was in a dreadful hurry and did the whole process in less than 24 hours....

I then did a small test, and thinned the High Gloss Pattern Coat with around 8 % Acetone ... then brushed it on ... MUCH better result ...   Might be worth a try, If you can not spray your plug...

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Zedok
Zedok
Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)
Group: Forum Members
Posts: 18, Visits: 115
Many thanks Hanaldo and Dravis for your comments and encouragements. At least my observations are normal and I have not f***ed up... yet.
 
I have ordered a set of orbital 240, 400 and 800 orbital discs which should make the job easier. 

Spraying is not an option at this point. Anyhow, I would have to take time and learn how to spay correctly. Might as well take that time and sand. The idea of thinning the Gloss resin with 8% acetone seems very appealing and I shall have a try on a small part of the the pattern.

Hanaldo, you mentioned: "Fortunately, it's easy to fill these little holes and sand smooth. " Do you mean filling them with additional gloss resin? 

Cheers,
Z
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Keep up the good work, you will come good in the end.

Do a bit then walk away and come back fresh.

I'm polishing three moulds and sanding two plugs at present, they are much smaller than your hull but quite tricky so I give them an hour then take a 10min rest and come back with fresh eyes, I want them perfect so am now down to 2000 grit paper before buffing.

will look trick when finished and you will feel 100% after doing it yourself.
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Yeah .. excellent advice that ... polishing and wet sanding should be done in between other jobs .. otherwise it becomes  (in the immortal words of the chartered accountant in Monty Python Cool) "Dull.. Dull. Dull... So DESPERATELY DULL ..."  LaughHehe

 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Zedok (29/06/2015)
Many thanks Hanaldo and Dravis for your comments and encouragements. At least my observations are normal and I have not f***ed up... yet.
 
I have ordered a set of orbital 240, 400 and 800 orbital discs which should make the job easier. 

Spraying is not an option at this point. Anyhow, I would have to take time and learn how to spay correctly. Might as well take that time and sand. The idea of thinning the Gloss resin with 8% acetone seems very appealing and I shall have a try on a small part of the the pattern.

Hanaldo, you mentioned: "Fortunately, it's easy to fill these little holes and sand smooth. " Do you mean filling them with additional gloss resin? 

Cheers,
Z


Yeh mate, just mix up a small amount of the gloss coat and and use a pop stick to dab it into the holes. Fill it proud of the surface so you can sand it down flat. Easy as. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search