Hi everyone, 
I've just uploaded a new video on my youtube-channel that might interest some of you 

https://youtu.be/EHLSzEmWzJs
(click link above)

All of this was done with materials from EC

http://www.talkcomposites.com/Uploads/Images/7530af1e-677b-4890-b8ab-c0d7.jpg


I did thes parts for a friend of mine called whaleboat, you can see the teaser of the boatproject on following link

https://www.youtube.com/watch?v=epHNYa6qc6s

Greetings MAT2COMPOSITES Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Replies
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
As you know I'm very new to this so when I call at EC I make sure to ask lots of questions,

 I used the Soft mesh and like how it follows the mould contours but as you know its hard to get back out,

Paul said try some bread wrap and so when I did the double part infusion I use the wrap in one and id say its 70% easier to remove the mesh.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
thanks for letting me know. heard about the technique and planned doing it. But while doing the lay up and after all the time put in it I never dared to do it because I get 100% perfect infusion every time and dont want to fail a part, but will try it on my next infusion Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
matthieutje65 - 10 Years Ago
VVS - 10 Years Ago
matthieutje65 - 10 Years Ago
AlessandroPA - 10 Years Ago
matthieutje65 - 10 Years Ago
carbonfibreworks - 10 Years Ago
redeye - 10 Years Ago
TomDesign - 10 Years Ago
Bonobo - 10 Years Ago
FLD - 10 Years Ago
Warren (Staff) - 10 Years Ago
VVS - 10 Years Ago
matthieutje65 - 10 Years Ago
VVS - 10 Years Ago
matthieutje65 - 10 Years Ago
Warren (Staff) - 10 Years Ago
matthieutje65 - 10 Years Ago
cr34tive - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search