Talk Composites - The Forum for Advanced Composites

How To: Carbon fiber and Nomex Honeycomb (Spacegrade)

http://www.talkcomposites.com/Topic17492.aspx

By matthieutje65 - 6/1/2015 8:54:48 PM

Hi everyone, 
I've just uploaded a new video on my youtube-channel that might interest some of you 

https://youtu.be/EHLSzEmWzJs
(click link above)

All of this was done with materials from EC

http://www.talkcomposites.com/Uploads/Images/7530af1e-677b-4890-b8ab-c0d7.jpg


I did thes parts for a friend of mine called whaleboat, you can see the teaser of the boatproject on following link

By matthieutje65 - 6/9/2015 8:55:41 PM

AlessandroPA (09/06/2015)
Hi Mathieu, I had a look at your video, very interesting and useful.
Can you make a brief of the materials you have used in the sequence with their characteristics, and the technique for each one (vacuum, infusion, hand lay up)? 

Thanks 

matthieutje65 (04/06/2015)
used the GC50 for UV protection so it doesn't need to be clearcoated at the end.
and was also good for a tack while positioning the carbon
The fiberglass was due to the fact I didn't had a 200g/m² cf at the moment Smile carbonfiber would ofcourse be better!


I'll add a "products used" in the description of the video soon. All materials are from Easycomposites so you should be able to find some characteristics and so on on their website then Wink