Hi guys,

How much do your various pre-pregs change thickness between uncured and cured states
Thanks.
Steve
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Steve,

When you measure the thickness of the uncured pre-preg if you put some pressure on the vernier to try to 'squash' the carbon fabric down somewhat then this measurement will be very close to the measurement that you'll get in a cured laminate. It does depend on the amount of pressure you're putting the laminate under but even this only makes a small difference. You should find the original vernier measurement will be within around 0.05mm.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search