John Rutter
John Rutter
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 27
Gents,
Total novice looking for advice. I am a novice car restorer (engine builds etc.) but lacking in bodywork skills. I have been lucky enough to purchase a Lambo with carbon fibre side skirts. They have been damaged by kerbs. I have just been quoted £4000 to have them repaired which seems nonsense. the damage is low down so I reckon the weave may not match perfectly but as it is dark it should not matter too much. Do you think this could be repaired using one of your kits, and if so which one should I purchase? Regards, John
Attachments
photo 1.JPG
(
622 views,
710.00 KB
)
photo 2.JPG
(
510 views,
665.00 KB
)
Reply
Like
4
Reply
Dravis
Dravis
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
uhhhh .. be careful Sounds a bit like you've been stung by the "Composites bug" --- It' a disease most detrimental to spare time and wallet, only one illness worse in that respect is a condition called "Armas Numeralis"
Not only does that make you poor, it also stunts your social acceptability, tends to make your views politically incorrect, and may in time turn you into a redneck
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Repairing a carbon fibre side skirt
John Rutter
-
10 Years Ago
Normal 0 false false false EN-GB X-NONE X-NONE...
Warren (Staff)
-
10 Years Ago
Many thanks Warren, will study your help guides and work out a plan.
John Rutter
-
10 Years Ago
Alternatively ... when the structural repairs have been completed, mark up "cut-lines" on the...
Dravis
-
10 Years Ago
Thanks Dravis, I like the idea of creating a 'feature line away from the damaged area. I will study...
John Rutter
-
10 Years Ago
The only problem with skinning sections of it, is getting an exact match, if the part was pre-preg...
Warren (Staff)
-
10 Years Ago
I do not think you'll be able to make an exact match to a specialized Pre-preg part, which is why I...
Dravis
-
10 Years Ago
I agree with Dravis' line of thinking. You will never be able to make a seamless repair, so why not...
Hanaldo
-
10 Years Ago
This might be an unorthodox approach but given its always going to look repaired if you try to match...
FLD
-
10 Years Ago
Many thanks for the reply. I like the idea of the feature and if it does not look well I will go for...
John Rutter
-
10 Years Ago
Don't wrap it. rather paint it in white like rest of the car. fake carbon looks terrible. on Lambo...
tomzi1234
-
10 Years Ago
Errrhmm .. :doze: ... Its NOT "Fake Carbon" The skirts are actually Carbon -kevlar items ......
Dravis
-
10 Years Ago
Guys, Just noticedyour replies, many thanks for them. I reckon I am going to try to repair with...
John Rutter
-
10 Years Ago
uhhhh .. be careful Sounds a bit like you've been stung by the "Composites bug" --- It' a disease...
Dravis
-
10 Years Ago
Previously i meant, don't wrap it so kind of vinyl. that i meant with fake carbon. repairing it...
tomzi1234
-
10 Years Ago
Yes I guessed that's what you meant. I need to trial a little before I venture to the car. John
John Rutter
-
10 Years Ago
just looked at the damage again, if it was me I would completely sand back the first ply, repair the...
scottracing
-
10 Years Ago
Thanks 'Scott racing' I will look in to that repair as with the other options. The quote was from a...
John Rutter
-
10 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search