By John Rutter - 5/25/2015 9:59:48 AM
Gents,
Total novice looking for advice. I am a novice car restorer (engine builds etc.) but lacking in bodywork skills. I have been lucky enough to purchase a Lambo with carbon fibre side skirts. They have been damaged by kerbs. I have just been quoted £4000 to have them repaired which seems nonsense. the damage is low down so I reckon the weave may not match perfectly but as it is dark it should not matter too much. Do you think this could be repaired using one of your kits, and if so which one should I purchase? Regards, John
|
By John Rutter - 6/5/2015 9:06:44 PM
Thanks 'Scott racing' I will look in to that repair as with the other options. The quote was from a 'you have a Lambo so you must be rich' type company. Which I am not!
John
|
|