Hi folks.

i have a car which a previous owner painted matt black, its not my choice, but it is a race car so spending a lot having it resprayed is a waste as it won't make it go any faster!

i want to mould the panels as spares, but in carbon, and hopefully replace all the panels with home-made carbon ones eventually, but can i take moulds from something that is painted with a matt paint or will it adversely affect the surface of the mould and will it tend to have more bite- so it won't release cleanly?

thanks
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
you can certainly take a mould off the surface, but you will need to wax and release it like any normal part and then spend the time sanding and polishing your mould to get the desired surface finish.
I would spend the time on the bodypanels by lacquering and buffing them up to give a much better surface finish.
Dogger
Dogger
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 5, Visits: 46
Thanks for that.

I thought the best solution would be to paint them, but it is going to take me a while to get it all done and the car will be in use during this time, so i didnt want to be running around with a patchwork car, plus i have to run sponsors stickers.

I guess i shouldn't be trying to do everything at once and risk compromising my mould
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
You will have problems in that you have to remove the sponsor vinyl stickers as they will come off when you gel coat, its reactive enough to fetch paint off so you need to work this into your build time.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Personally I don't think it's an issue. Spray PVA as a release agent and there will be very minimal sanding needed to make the moulds glossy. Quick flat with 1200 then compound would do it. 

Certainly there I merit in the idea of perfecting the patterns before making the moulds, but are you going to be selling these panels? Will the moulds be production moulds that you're gonna pull 50 parts from? If not, I'd question the worth of spending a lot of time and money getting the patterns perfect when it would be a lot cheaper and a lot simpler to just polish up the moulds. 

Of course if the current paint is in pretty bad condition, then it would probably be worth getting them fixed up and painted. If it is in good condition and just has a matt finish then I say go ahead and make the moulds. 
Dogger
Dogger
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 5, Visits: 46
Thanks again for the replies.
I realise i'll have to take the stickers off, i'm a little concerned they might try and take some of the paint with them as i have a funny feeling it might be rattle can paint, so it could be thin and generally rubbish.

I can't imagine i will be doing multiple pulls from the moulds, but if it is spray can paint i can just imagine some of the paint coming away and spoiling the mould, or at least needing a lot of re-work to finish the mould. 

Hanaldo- i think you could be right- i'll just have to be generous with the release agents and then finish the mould afterwards.
thanks
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yep, PVA is your friend. Spray it on like it's a paint, get a nice thick application. You won't have any issues. If the paint is a really bad job then it may come off the part and stay in the mould, but as long as you've got PVA it'll come off with a quick blast with a high pressure washer. 