Hello,

I would like to cut through various carbon fiber panels with a range of EasyCell75 foam core (3mm, 10mm, 20mm). Will a dremel cutting tool be adequate for cutting through these panels?

Thank you
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Hi Ahmedgehad,

The 32mm rotary disc with a dremal cuts like a champ https://www.easycomposites.co.uk/permagrit-32mm-rotary-disc-with-arbor



Have used mine quite a lot ...



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Just keep the carbon dust well away from the electric motor of the dremel!! Have had 4 of them go bang in my hand, never a pleasant sensation. 
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Yup good advice Hanaldo!

My little cordless Dremal is suffering from living in an atmosphere of carbon dust Sad
Won't be long till I treat myself to decent https://www.easycomposites.co.uk/tools/Dremel-Fortiflex-9100-Heavy-Duty-Flexshaft-and-Hanging-Motor.aspx?117585 Wink




And use a decent quality mask, eye protection, ear protection, gloves, codpeice !



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search