Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
Cutting carbon fiber and core panel
http://www.talkcomposites.com/Topic17250.aspx
By Ahmedgehad
-
5/20/2015 9:17:13 PM
Hello,
I would like to cut through various carbon fiber panels with a range of EasyCell75 foam core (3mm, 10mm, 20mm). Will a dremel cutting tool be adequate for cutting through these panels?
Thank you
By davro
-
5/21/2015 1:40:39 PM
Yup good advice Hanaldo!
My little cordless Dremal is suffering from living in an atmosphere of carbon dust
Won't be long till I treat myself to decent
https://www.easycomposites.co.uk/tools/Dremel-Fortiflex-9100-Heavy-Duty-Flexshaft-and-Hanging-Motor.aspx?117585
And use a decent quality mask, eye protection, ear protection, gloves, codpeice !