Hello from really sunny England, I could do with some help guys, could anybody on here tell me if it is possible to create resin infused MDF board with a metallic substance in the composite.  I am working on a project and am interested to know if it would be possible to add magnetic particulates to the resin before infusing the MDF.  And if so, would this be a costly affair on top of the resin infusion ie would your require different machinery etc???

Thanks in anticipation.

Robbie
Edited 10 Years Ago by DemonFlooring
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
HI Robbie,
I'm a little unclear what you actually want to do, how do you intend on infusing MDF? It's dense & non porous, you could surface coat it but that's about it.

Chris