You CAN get MDF to absorb quite a lot of infusion resin, just like wood can be "stabilized" by soaking it in Infusion Resin in a vacuum.  I use that a lot to make "stabilized wood" for knife handles e.t.c.

BUT! .... You would need EXTREMELY fine iron particles to get them to "follow the resin" into the MDF.. I've had even pigments stay on the surface of certain types of wood, effectively being "filtered" from the resin by the size of the pores.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
DemonFlooring
DemonFlooring
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 3, Visits: 75
Interesting pointy, thank you
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Ah, see I read that and assumed you meant infuse a laminate on TOP of the mdf... I can't see you successfully infusing a piece of mdf at all, let alone with any filler powders. Mdf may be porous, but it is already a matrix of its own... There is no path to accommodate flow like there is in a woven fabric. 
DemonFlooring
DemonFlooring
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 3, Visits: 75
Thanks for the comments guys, Chris, I am confident MDF is quite porous when unsealed.  I am very much liking the idea of iron powder.  Thank you guys.
ChrisR
ChrisR
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
HI Robbie,
I'm a little unclear what you actually want to do, how do you intend on infusing MDF? It's dense & non porous, you could surface coat it but that's about it.

Chris
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Like said you will need to do some tests.

I'm not sure of its magnetic properties compared to iron as a powder but iron oxide is used as a pigment in plastics manufacturing,

this would be much finer than iron so would disperse better.

We sell iron oxide and iron chrome at work so I maybe able to supply information if needed.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I have never actually tried this so I don't know whether it would work or not, but in theory you could add iron powder to the resin to create a dielectromagnetic. There are 2 possible issues I can see though. 1 is that resin is obviously not magnetic, and therefore you are relying on the particles of iron powder to create the magnetism that you want. This means you need an iron powder that is quite pure, as impurities like carbon etc. will affect the magnetic field. 

The second issue is that you want to infuse. The amount of iron powder that you would need to add to build the level of magnetism that you desire may quite possibly raise the viscosity of the resin to a level where it won't infuse. To combat this, I would be finding the lowest viscosity resin that you can get. 

Perhaps some of the Easy Composites staff can provide some better insight, but I have a feeling this is going to involve a degree of experimentation to work out how much iron powder you would need to add as well as how much it affects your viscosity and if it can be infused. 
DemonFlooring
DemonFlooring
Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)Forum Member (39 reputation)
Group: Forum Members
Posts: 3, Visits: 75
Hello from really sunny England, I could do with some help guys, could anybody on here tell me if it is possible to create resin infused MDF board with a metallic substance in the composite.  I am working on a project and am interested to know if it would be possible to add magnetic particulates to the resin before infusing the MDF.  And if so, would this be a costly affair on top of the resin infusion ie would your require different machinery etc???

Thanks in anticipation.

Robbie
Edited 11 Years Ago by DemonFlooring