Loss of vacuum


Author
Message
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi all,

I have been trying to pull vac on a panel in making and I can pull but not hold vac.

I started off with just a bag around the top face, edge taped, and after an hour or more of no joy put a second bag around the whole mould and first bag,

this still will not hold vac SO is it simply a case of poor bags (pin holes) or have I lost the plot!
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Haha, ive spent the best part of two days going over it so normality says it is in the bag somewhere.

Its no real problem as I'm new to all this so cutting my teeth.

the more issues I have the more I learn, step curve but very interesting all the same.