what best Laquer for carbon stuff?
what best Laquer for carbon stuff?
Post Reply
Like
2
what best Laquer for carbon stuff?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Guys any feedback so have very hard surface.
Reply
Like
2
Reply
Dravis
Dravis
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
I have used marine 2-component polyurethane clear coat ... Very strong stuff ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
what best Laquer for carbon stuff?
TomDesign
-
10 Years Ago
I have used marine 2-component polyurethane clear coat ... Very strong stuff ..
Dravis
-
10 Years Ago
Dravis- please link. need heating? hard surface from scratches?
TomDesign
-
10 Years Ago
http://www.marineware.com/index.php?option=com_content&view=category&id=88:durepox-clear&Itemid=88&l...
ChrisR
-
10 Years Ago
Yep ChrisR ... thats the stuff ... :D
Dravis
-
10 Years Ago
one note on this stuff is that you need to do any finishing within a couple of days, any more than...
ChrisR
-
10 Years Ago
i just bought 2k polurethane clear coat for yachts. now testing hope it work.
TomDesign
-
10 Years Ago
Same stuff I use too! Very tough stuff. Definitely need to do finishing work the next day ideally,...
Hanaldo
-
10 Years Ago
going to see today evening that be 24 hours how that work i hope that not be trash like car clear...
TomDesign
-
10 Years Ago
any idea on this to cover wrapped parts in carbon https://www.youtube.com/watch?v=O7qyKCTwiMI
TomDesign
-
10 Years Ago
[quote][b]TomDesign (25/04/2015)[/b][hr]any idea on this to cover wrapped parts in carbon...
Fasta
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search