Hi all,

I want to make a mould of an original car part that would be expensive to replace if I damaged it. Is there any way around this? I've tried using 3m 1080 vinyl wrap in the past on cheaper parts from the same car but that didn't protect the original part at all.

What methods has everyone used to minimise damage to the original part they're making moulds of?
Replies
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I have never had any problems with the original paint on painted plastic bike parts or car parts, when using careful waxing and epoxy gelcoat..
maybe I will get problems showing up when I start using the Unimould system. Whistling

Best try on an old part first ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Dravis (08/04/2015)
I have never had any problems with the original paint on painted plastic bike parts or car parts, when using careful waxing and epoxy gelcoat..
maybe I will get problems showing up when I start using the Unimould system. Whistling

Best try on an old part first ..


One things for sure the uni system hates rattle can paint, i know i spent 2 hours scraping the paint off the mould! D'oh! 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
cpalada - 10 Years Ago
Hanaldo - 10 Years Ago
cpalada - 10 Years Ago
Hanaldo - 10 Years Ago
cpalada - 10 Years Ago
Dravis - 10 Years Ago
VVS - 10 Years Ago
cpalada - 10 Years Ago
Hanaldo - 10 Years Ago
Hanaldo - 10 Years Ago
VVS - 10 Years Ago
Hanaldo - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search