Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
What is the best way to cure a laminate of carbon fiber?
What is the best way to cure a laminate of carbon fiber?
Post Reply
Like
2
What is the best way to cure a laminate of carbon fiber?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Pakito
Pakito
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 33
What is the best way to cure a laminate of carbon fiber and what parts are more perfect?
- Drying at room temperature
- Oven
- Vacuum
Best Regards,
Jorge Ferreira
Reply
Like
2
Replies
Pakito
Pakito
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 33
A vacuum pump is to suck the air inside the bags suitable for the piece is "stuck" in the plastic, right?
Reply
Like
3
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Hi,
I think you are getting a little confused over things. The best bet is to have a read of these links first...
http://www.ecfibreglasssupplies.co.uk/t-WetLayUpwithVacuumBag.aspx
Pages 48 onwards of this one:
http://www.gurit.com/files/documents/guide-to-compositesv5webpdf.pdf
Chris
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
What is the best way to cure a laminate of carbon fiber?
Pakito
-
10 Years Ago
There is no best way other than what works best for you or your product.
Fasta
-
10 Years Ago
A vacuum pump is to suck the air inside the bags suitable for the piece is "stuck" in the plastic,...
Pakito
-
10 Years Ago
Hi, I think you are getting a little confused over things. The best bet is to have a read of these...
ChrisR
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search