What is the best way to cure a laminate of carbon fiber?


Author
Message
Pakito
Pakito
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 33
What is the best way to cure a laminate of carbon fiber and what parts are more perfect? 

- Drying at room temperature 
- Oven 
- Vacuum 

Best Regards, 
Jorge Ferreira
Replies
Pakito
Pakito
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 33
A vacuum pump is to suck the air inside the bags suitable for the piece is "stuck" in the plastic, right?
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Hi,
I think you are getting a little confused over things. The best bet is to have a read of these links first...