After cured resin in the carbon fiber can customize it with print vinyl?
Can I go back to put another layer of resin over the vinyl for you to have protection and without gaining air bubbles?

Best Regards,
Jorge Ferreira
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Clear coating is best in this situation.  However we always recommend testing on a bit of scrap first as sometimes the vinyl curls or if its been printed, the inks run.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search